MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmocap® 11 A Epoxy Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Epoxy

Material Notes: Desmocap 11 A is a branched polymer with ether and urethane groups; contains crosslinking, blocked isocyanate groups. It is suitable as a raw material for use in the flexibilisation of epoxy resins and the formulation of flexible coatings and sealing compounds.

Properties / Applications: Desmocap 11 A can be used to formulate curable, liquid, solvent-free polyurethane systems. The polyamines normally used with epoxy resins are suitable curing agents. The best results are obtained with cycloaliphatic diamines, e.g. Laromin® C 260, Ancamine® XT, TCD-Diamin, xylene diamine, etc. When combined with epoxy resins, Desmocap 11 A takes on the function of a reactive flexibiliser. As with any product, use of Desmocap 11 A in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Solids Content 100 %100 %
Viscosity 60000 - 120000 cP60000 - 120000 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 210 °C410 °FCleveland Open Cup
 
Descriptive Properties
AppearanceClear, slightly yellow liquid
Color<200Hazen
Content2.75-3.2%Blocked NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Atom Adhesives AA-BOND F110 Epoxy Adhesive
Armstrong A-1/A Epoxy Adhesive
Aremco Aremco-Bond™ 2330 High Performance Epoxide
Aremco Aremco-Bond™ 2300 High Performance Epoxide

PCOVEST0277 / 202060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.