MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® XG-FKGS6 PA6-GF30 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Flame Retardant, Halogen free

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³dry; ISO 1183
Moisture Absorption 1.70 %1.70 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inSim. To ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 85.0 MPa12300 psicond; ISO 527-1/-2
 135 MPa19600 psidry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %dry; ISO 527-1/-2
 3.7 %3.7 %cond; ISO 527-1/-2
Tensile Modulus 7.10 GPa1030 ksicond; ISO 527-1/-2
 11.5 GPa1670 ksidry; ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 Vcond; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °Fdry; ISO 75-1/-2
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
IEC 60695-11-10
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
Glow Wire Ignition Temperature  775 °C
@Thickness 1.60 mm
1430 °F
@Thickness 0.0630 in
IEC 60695-2-13
 775 °C
@Thickness 1.00 mm
1430 °F
@Thickness 0.0394 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
Dry; IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
Dry; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® Ultraflow K-FKGS6/B PA6-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
Domo TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Envalior Akulon® K225-KS PA6 FR(30), Dry, Flame Retardant, Heat Stabilized
Envalior Novamid® 1010GN8-30 NAT PA6-GF30 FR

PDSM9705 / 161326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.