MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 1171 materials in the category Nylon 6, 30% Glass Fiber Filled. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 1171 Results -- Page of 24 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Nylon 6, 30% Glass Fiber Filled
 2Aclo Accutech Nylon 6 NY0730G30L Glass Reinforced
 3Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
 4Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Conditioned, 25% Glass Filled
 5Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
 6Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Conditioned, 30% Glass Filled
 7Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled
 8Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Conditioned, 30% Glass Filled
 9Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled
 10Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Conditioned, 30% Glass Filled
 11Akro-Plastic Akromid® B3 GF 30 2 GIT (4618) PA 6 Dry, 30% Glass Filled
 12Akro-Plastic Akromid® B3 GF 30 2 GIT (4618) PA 6 Conditioned, 30% Glass Filled
 13Akro-Plastic Akromid® B3 GK 30 1 L black (4674) PA 6 Dry, 30% Glass Filled
 14Akro-Plastic Akromid® B3 GK 30 1 L black (4674) PA 6 Conditioned, 30% Glass Filled
 15Akro-Plastic Akromid® A3 GF 30 4 L black (4678) PA 6 Dry, 30% Glass Filled
 16Akro-Plastic Akromid® A3 GF 30 4 L black (4678) PA 6 Conditioned, 30% Glass Filled
 17Akro-Plastic Akromid® S3 GF 30 1 L black (4657) PA 6 Dry, 30% Glass Filled
 18Akro-Plastic Akromid® S3 GF 30 1 L black (4657) PA 6 Conditioned, 30% Glass Filled
 19Akro-Plastic Akromid® B3 GF 25 1 black PA 6 Dry, 25% Glass Filled, Heat Stabilized
 20Akro-Plastic Akromid® B3 GF 25 1 black PA 6 Conditioned, 25% Glass Filled, Heat Stabilized
 21Akro-Plastic Akromid® B3 GF 25 1 L black (4637) PA 6 Dry, 25% Glass Filled, Heat Stabilized
 22Akro-Plastic Akromid® B3 GF 25 1 L black (4637) PA 6 Conditioned, 25% Glass Filled, Heat Stabilized
 23Akro-Plastic Akromid® B3 GF 25 1 natural (2463) PA 6 Dry, 25% Glass Filled, Heat Stabilized
 24Akro-Plastic Akromid® B3 GF 25 1 natural (2463) PA 6 Conditioned, 25% Glass Filled, Heat Stabilized
 25Akro-Plastic Akromid® B3 GF 25 black PA 6 Dry, 25% Glass Filled
 26Akro-Plastic Akromid® B3 GF 25 black PA 6 Conditioned, 25% Glass Filled
 27Akro-Plastic Akromid® B3 GF 30 1 black PA 6 Dry, 30% Glass Filled, Heat Stabilized
 28Akro-Plastic Akromid® B3 GF 30 1 black PA 6 Conditioned, 30% Glass Filled, Heat Stabilized
 29Akro-Plastic Akromid® B3 GF 30 1 L black (4365) PA 6 Dry, 30% Glass Filled, Heat Stabilized
 30Akro-Plastic Akromid® B3 GF 30 1 L black (4365) PA 6 Conditioned, 30% Glass Filled, Heat Stabilized
 31Akro-Plastic Akromid® B3 GF 30 1 natural PA 6 Dry, 30% Glass Filled, Heat Stabilized
 32Akro-Plastic Akromid® B3 GF 30 1 natural PA 6 Conditioned, 30% Glass Filled, Heat Stabilized
 33Akro-Plastic Akromid® B3 GF 30 1 XL black (4366) PA 6 Dry, 30% Glass Filled, Heat Stabilized
 34Akro-Plastic Akromid® B3 GF 30 1 XL black (4366) PA 6 Conditioned, 30% Glass Filled, Heat Stabilized
 35Akro-Plastic Akromid® B3 GF 30 2 RM-D black (3424) PA 6 + ABS Dry, 30% Glass Filled
 36Akro-Plastic Akromid® B3 GF 30 2 RM-D black (3424) PA 6 + ABS Conditioned, 30% Glass Filled
 37Akro-Plastic Akromid® B3 GF 30 4 RM-M black (3476) PA 6 Dry, 30% Glass Filled
 38Akro-Plastic Akromid® B3 GF 30 4 RM-M black (3476) PA 6 Conditioned, 30% Glass Filled
 39Akro-Plastic Akromid® B3 GF 30 9 RM-M natural (3292) PA 6 Dry, 30% Glass Filled
 40Akro-Plastic Akromid® B3 GF 30 9 RM-M natural (3292) PA 6 Conditioned, 30% Glass Filled
 41Akro-Plastic Akromid® B3 GF 30 black PA 6 Dry, 30% Glass Filled
 42Akro-Plastic Akromid® B3 GF 30 black PA 6 Conditioned, 30% Glass Filled
 43Akro-Plastic Akromid® B3 GF 30 RM-M natural (3291) PA 6 Dry, 30% Glass Filled
 44Akro-Plastic Akromid® B3 GF 30 RM-M natural (3291) PA 6 Conditioned, 30% Glass Filled
 45Akro-Plastic Akromid® B3 GF 25 1 L natural (4781) PA6 + PP, Dry, 25% Glass Filled
 46Akro-Plastic Akromid® B3 GF 25 1 L natural (4781) PA6 + PP, Conditioned, 25% Glass Filled
 47Akro-Plastic Akromid® B3 GF 30 1 L black (4491) PA6 + PP, Dry, 30% Glass Filled
 48Akro-Plastic Akromid® B3 GF 30 1 L black (4491) PA6 + PP, Conditioned, 30% Glass Filled
 49Akro-Plastic Akromid® B3 GF 30 1 L natural (4684) PA6 + PP, Dry, 30% Glass Filled
 50Akro-Plastic Akromid® B3 GF 30 1 L natural (4684) PA6 + PP, Conditioned, 30% Glass Filled
 
Found 1171 Results -- Page of 24 -- [Prev Page] [Next Page] --  view per page

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.