MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Esprix Ketoprix™ EKT63 (Natural) Thermoplastic Aliphatic Polyketone, Low melt flow IM Grade
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Ketoprix™ EK63 and EKT63 resins are thermoplastic aliphatic polyketones containing a 1,4-diketone backbone structure. They are produced from ethylene, propylene and CO with perfectly alternating olefin and CO monomers in the backbone. These natural resins are low MF IM resins and are well suited for IM parts and lightly filled compounds. Ketoprix™ EK63 and EKT63 have excellent flow properties and are used in E&E, CAM, Auto and Industrial End Uses. These resins can also be used in small diameter pipe & profile extrusion applications.

Information provided by Esprix Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³
Density 1.24 g/cc0.0448 lb/in³ASTM D 792
Moisture Absorption 0.450 %
@Temperature 23.0 °C
0.450 %
@Temperature 73.4 °F
60% RH, wt%; ASTM D570
Viscosity Test 210 cm³/g2.10 dl/gLimiting Viscosity
Molecular Weight 276000 g/mol276000 g/molWeight Average
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm0.018 - 0.020 in/inASTM D 955
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 240 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 464 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D 785
Tensile Strength 65.0 MPa
@Temperature 23.0 °C
9430 psi
@Temperature 73.4 °F
ASTM D 638
Elongation at Break 250 %250 %Nominal; ASTM D 638
Tensile Modulus 1.60 - 2.20 GPa
@Temperature 23.0 °C
232 - 319 ksi
@Temperature 73.4 °F
ASTM D 638
Flexural Strength 60.0 MPa
@Temperature 23.0 °C
8700 psi
@Temperature 73.4 °F
ASTM D 790
Flexural Modulus 1.60 GPa
@Temperature 23.0 °C
232 ksi
@Temperature 73.4 °F
ASTM D 790
Charpy Impact, Notched 2.00 - 5.00 J/cm²
@Temperature 23.0 °C
9.52 - 23.8 ft-lb/in²
@Temperature 73.4 °F
ASTM D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D 257
Dielectric Strength 17.0 kV/mm432 kV/inASTM D 149
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 84.0 J/g36.1 BTU/lbtypical molded material
 227 J/g97.7 BTU/lb100% crystalline material
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°F
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°F
Specific Heat Capacity  1.84 J/g-°C
@Temperature 50.0 °C
0.440 BTU/lb-°F
@Temperature 122 °F
heating rate = 20°C/min
 2.62 J/g-°C
@Temperature 170 °C
0.626 BTU/lb-°F
@Temperature 338 °F
heating rate = 20°C/min
 2.68 J/g-°C
@Temperature 250 °C
0.641 BTU/lb-°F
@Temperature 482 °F
heating rate = 20°C/min
Melting Point 220 °C428 °FASTM D 1525
Crystallization Temperature 178 °C352 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FASTM D 648
Glass Transition Temp, Tg 15.0 °C59.0 °F
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Chloride, AlCl3
Yparex 8305 Polyolefin Adhesive Resin (European Grade)
Total Lacqtene® 2001 TBK 46 HDPE pipe
Polyglycolic Acid (PGA)
Lithium Nitrate, LiNO3

PESPR905 / 217559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.