MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Lacqtene® 2001 TBK 46 HDPE pipe  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process.

LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and potable water.

LACQTENE® 2001 TBK 46 is best processed between 190 and 230°C.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ISO 1183
Viscosity 1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Environmental Stress Crack Resistance >= 700 hour>= 700 hourASTM D1693
Oxidative Induction Time (OIT) >= 20 min>= 20 min210°C; EN 728
 >= 30 min>= 30 min200°C; EN 728
Carbon Black Loading 2.0 - 2.5 %2.0 - 2.5 %ISO 6964
Melt Flow  0.10 g/10 min
@Load 2.16 kg
0.10 g/10 min
@Load 4.76 lb
ISO 1133
 0.45 g/10 min
@Load 5.00 kg
0.45 g/10 min
@Load 11.0 lb
ISO 1133
High Load Melt Index 12 g/10 min
@Load 21.6 kg
12 g/10 min
@Load 47.6 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161DIN 53505
Tensile Strength at Break 34.0 MPa4930 psiISO 527
Tensile Strength, Yield 24.0 MPa3480 psiISO 527
Elongation at Break >= 700 %>= 700 %ISO 527
Elongation at Yield 9.0 %9.0 %ISO 527
Modulus of Elasticity 1.05 GPa152 ksiISO 178
Flexural Modulus 1.00 GPa145 ksiASTM D 790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 93
Dielectric Constant 2.4
@Frequency 1000 Hz
2.4
@Frequency 1000 Hz
IEC 250
Dielectric Strength 18.0 kV/mm457 kV/inIEC 243
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 175 J/g75.3 BTU/lbDSC
CTE, linear 160 µm/m-°C
@Temperature 20.0 °C
88.9 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 2.00 J/g-°C0.478 BTU/lb-°FDSC
 2.60 J/g-°C
@Temperature 150 °C
0.621 BTU/lb-°F
@Temperature 302 °F
DSC
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FDIN 52612
 0.200 W/m-K
@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 302 °F
DIN 52612
Melting Point 128 - 131 °C262 - 268 °Fcrystalline; DSC
Vicat Softening Point 127 °C261 °FISO 306
 
Descriptive Properties
Food StatusConforms to both European and American Food contact regulations.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Chloride, AlCl3
Esprix Ketoprix™ EKT63 (Natural) Thermoplastic Aliphatic Polyketone, Low melt flow IM Grade
Lithium Nitrate, LiNO3
Polyglycolic Acid (PGA)
Yparex 8305 Polyolefin Adhesive Resin (European Grade)

PFINAP130 / 38713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.