MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lacqtene® 2001 TBK 46 HDPE pipe  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process.

LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and potable water.

LACQTENE® 2001 TBK 46 is best processed between 190 and 230°C.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccISO 1183
Viscosity 1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
ATOFINA research test
Environmental Stress Crack Resistance >= 700 hourASTM D1693
Oxidative Induction Time (OIT) >= 20 min210°C; EN 728
 >= 30 min200°C; EN 728
Carbon Black Loading 2.0 - 2.5 %ISO 6964
Melt Flow 0.10 g/10 min
@Load 2.16 kg
ISO 1133
 0.45 g/10 min
@Load 5.00 kg
ISO 1133
High Load Melt Index 12 g/10 min
@Load 21.6 kg
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61DIN 53505
Tensile Strength at Break 34.0 MPaISO 527
Tensile Strength, Yield 24.0 MPaISO 527
Elongation at Break >= 700 %ISO 527
Elongation at Yield 9.0 %ISO 527
Modulus of Elasticity 1.05 GPaISO 178
Flexural Modulus 1.00 GPaASTM D 790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 93
Dielectric Constant 2.4
@Frequency 1000 Hz
IEC 250
Dielectric Strength 18.0 kV/mmIEC 243
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 175 J/gDSC
CTE, linear 160 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 2.00 J/g-°CDSC
 2.60 J/g-°C
@Temperature 150 °C
DSC
Thermal Conductivity 0.400 W/m-KDIN 52612
 0.200 W/m-K
@Temperature 150 °C
DIN 52612
Melting Point 128 - 131 °Ccrystalline; DSC
Vicat Softening Point 127 °CISO 306
 
Descriptive Properties
Food StatusConforms to both European and American Food contact regulations.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Chloride, AlCl3
Esprix Ketoprix™ EKT63 (Natural) Thermoplastic Aliphatic Polyketone, Low melt flow IM Grade
Lithium Nitrate, LiNO3
Polyglycolic Acid (PGA)
Yparex 8305 Polyolefin Adhesive Resin (European Grade)

PFINAP130 / 38713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.