MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-17365 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-17365 is a high performance thermoplastic elastomer, available in NAT and colors, specifically designed for healthcare and medical applications. Medalist MD-17365 is a medium hardness, low density, halogen-free grade that can be sterilized and is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Colorability; Good Flexibility; Good Moldability; Halogen Free; Low Density; Low Flow; Medium Hardness; Low Specific Gravity; Radiation (Gamma) Resistant; Radiation Sterilizable; Resilient; Slip; Without Fillers

Uses: Bladders; Bushings; Connectors; Disposable Hospital Goods; Flexible Grips; Grommets; Handles; Knobs; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement; Seals

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  66
@Time 5.00 sec
66
@Time 0.00139 hour
Injection Molded; ASTM D2240
 68
@Time 1.00 sec
68
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 11.7 MPa1700 psiASTM D412
Tensile Stress at Strain  2.48 MPa
@Strain 100 %
360 psi
@Strain 100 %
ASTM D412
 4.48 MPa
@Strain 300 %
650 psi
@Strain 300 %
ASTM D412
Elongation at Break 750 %750 %ASTM D412
Compression Set  16 %
@Temperature 22.8 °C,
Time 79200 sec
16 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 84 %
@Temperature 70.0 °C,
Time 79200 sec
84 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 193 °C340 - 380 °FMelt, Injection
Rear Barrel Temperature 127 - 149 °C260 - 300 °FInjection
Middle Barrel Temperature 138 - 160 °C280 - 320 °FInjection
Front Barrel Temperature 149 - 171 °C300 - 340 °FInjection
Nozzle Temperature 171 - 193 °C340 - 380 °FInjection
Zone 1 138 - 149 °C280 - 300 °FExtrusion
Zone 2 149 - 160 °C300 - 320 °FExtrusion
Zone 3 160 - 182 °C320 - 360 °FExtrusion
Zone 4 160 - 182 °C320 - 360 °FExtrusion
Zone 5 171 - 193 °C340 - 380 °FExtrusion
Die Temperature 182 - 204 °C360 - 400 °FExtrusion
Mold Temperature 21.1 - 37.8 °C70.0 - 100 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-12362 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12160H Thermoplastic Elastomer
Teknor Apex Medalist® MD-32265 Thermoplastic Elastomer
Teknor Apex Medalist® MD-17270 Thermoplastic Elastomer
Teknor Apex Medalist® MD-50357 Thermoplastic Elastomer

PTEKNQ0713 / 237204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.