MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Elastamax™ HTE 3080 Polyvinyl Chloride + NBR (PVC+NBR)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons and oils, offer excellent weatherability, and are an economical alternative to thermoset rubber and other more costly thermoplastic elastomers.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Melt Flow 0.46 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.46 g/10 min
@Load 11.0 lb,
Temperature 374 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 808015 sec; ASTM D2240
Tensile Strength at Break 19.3 MPa2800 psiType IV, 510 mm/min; ASTM D638
Tensile Stress at Strain  8.94 MPa
@Strain 100 %
1300 psi
@Strain 100 %
Type IV, 510 mm/min; ASTM D638
 16.0 MPa
@Strain 300 %
2320 psi
@Strain 300 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 390 %390 %Type IV, 510 mm/min; ASTM D638
Tear Strength 57.6 kN/m329 pliDie C, 510 mm/min; ASTM D624
Compression Set  46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395A
 52 %
@Temperature 100 °C,
Time 79200 sec
52 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395A
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -49.0 °C-56.2 °FASTM D746
 
Descriptive Properties
AppearanceNatural Color
FeaturesGeneral Purpose
FormsPellets
Generic MaterialPVC+NBR
Generic NamePolyvinyl Chloride + NBR (PVC+NBR)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitriflex N-7411 NBR / PVC
Avient ProFlex™ MB NV866/20 Nitrile/PVC Elastomer (NBR/PVC) Compound
Avient Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR)
Armacell Monarch® F-06931 (Gray) NBR/PVC Foam
Armacell Monarch® F-06903 (Gray) NBR/PVC Foam

PH0POL0456 / 145025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.