MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nitriflex N-7411 NBR / PVC
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Excellent processability in transfer and injection processes. Indicated for applications that require good resistance to oils and fuels.

Applications: low hardness printing rolls, low hardness goods, hose covers, mould goods.

Information provided by Dax Resinas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.00 - 0.70 %0.00 - 0.70 %Method B-003; ASTM D5668
Mooney Viscosity 50 - 58
@Temperature 100 °C
50 - 58
@Temperature 212 °F
MML1+4, Method B-002; ASTM D1646
 
Descriptive Properties
AppearanceYellow sheets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ HTE 3080 Polyvinyl Chloride + NBR (PVC+NBR)
Avient ProFlex™ MB NV866/20 Nitrile/PVC Elastomer (NBR/PVC) Compound
Nitriflex N-7220 NBR / PVC
Nitriflex N-6420 NBR / PVC
Avient ProFlex™ MB NP70/30P Nitrile/PVC Elastomer (NBR/PVC) Compound

PDAX034 / 29459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.