MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® K224-G6-FC BK00001 PA6-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Food Contact Grade

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³dry; ISO 1183
Water Absorption 6.3 %6.3 %Sim. To ISO 62
Moisture Absorption 1.90 %1.90 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 110 MPa16000 psicond; ISO 527-1/-2
 180 MPa26100 psidry; ISO 527-1/-2
Elongation at Break 3.5 %3.5 %dry; ISO 527-1/-2
 7.0 %7.0 %cond; ISO 527-1/-2
Tensile Modulus 6.00 GPa870 ksicond; ISO 527-1/-2
 9.50 GPa1380 ksidry; ISO 527-1/-2
Flexural Strength 235 MPa34100 psidry; ISO 178
Flexural Modulus 8.60 GPa1250 ksidry; ISO 178
Charpy Impact Unnotched  7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
cond; ISO 179/1eU
 7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eU
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eA
 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
cond; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmcond; IEC 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmdry; IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmcond; IEC 60093
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
dry; IEC 60250
 3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
dry; IEC 60250
 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
cond; IEC 60250
 20
@Frequency 100 Hz
20
@Frequency 100 Hz
cond; IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/incond; IEC 60243-1
 30.0 kV/mm762 kV/indry; IEC 60243-1
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
dry; IEC 60250
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
dry; IEC 60250
 0.12
@Frequency 1e+6 Hz
0.12
@Frequency 1e+6 Hz
cond; IEC 60250
 0.30
@Frequency 100 Hz
0.30
@Frequency 100 Hz
cond; IEC 60250
Comparative Tracking Index 600 V600 Vcond; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°Fdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C38.9 µin/in-°Fdry; ISO 11359-1/-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °Fdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °Fdry; ISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® S 4090 G6 30% Glass Filled PBT
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled
Celanese Zytel® 101 NC010 PA66
Envalior Akulon® K224-G6 PA6-GF30, Conditioned, 30% Glass Filled
EMS-Grivory Grilon® BG-30 EC PA6-GF30

PDSM9720 / 161341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.