MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Matrix 999241 Composite Syntactic Foam
Categories: Other Engineering Material; Composite Core Material

Material Notes: Composite syntactic materials made from a combination of microspheres, liquid epoxy resins (matrix material) and re-enforcing fillers.

Information provided by Matrix Composites & Engineering

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psiASTM D1623
Tensile Modulus 4.50 GPa653 ksiASTM D1623
Compressive Strength 130 MPa18900 psiASTM D1621
Compressive Modulus 5.20 GPa754 ksiASTM D1621
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.7 µm/m-°C7.61 µin/in-°FASTM E831-03
Thermal Conductivity 0.168 W/m-K1.17 BTU-in/hr-ft²-°FASTM C518-04
 
Descriptive Properties
Service Depth5000 m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy
E-Glass Fiber, Generic
Lord Adhesives Circalok™ 6715 Silicone Encapsulant
Synfoam® HT-14 Syntactic Foam
E-CRGlas® Fiber

PMATRIX04 / 185389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.