MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Circalok™ 6715 Silicone Encapsulant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Circalok™ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature properties. It is the ideal product for potting and encapsulating densely packed components and for making flexible molds.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc
@Temperature 25.0 °C
1.25 g/cc
@Temperature 77.0 °F
Viscosity 14000 cP
@Temperature 25.0 °C
14000 cP
@Temperature 77.0 °F
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535
Tensile Strength, Yield 1.72 MPa
@Temperature 25.0 °C
250 psi
@Temperature 77.0 °F
Elongation at Yield 160 %160 %
Tear Strength 4.38 kN/m25.0 pliDie B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm
@Temperature 25.0 °C
1.00e+14 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 3.5
@Temperature 25.0 °C
3.5
@Temperature 77.0 °F
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.020
@Frequency 100000 Hz,
Temperature 25.0 °C
0.020
@Frequency 100000 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.40 µm/m-°C0.778 µin/in-°F
Thermal Conductivity 0.346 W/m-K2.40 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -100 °C-148 °FIntermittent
 -80.0 °C-112 °FContinuous
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ SC-102 Unfilled Silicone Encapsulant
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
Matrix 999241 Composite Syntactic Foam
Lord Adhesives Thermoset™ SC-309 Thermally Conductive Silicone Encapsulating System
Lord Adhesives Thermoset™ SC-300M Silicone Gel Encapsulant

PLORD060 / 86068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.