ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Injection Molded
Material Notes:
Data Provided by Exxon Chemical Canada.
Characteristics: Medium Flow, Good Stiffness, Good Impact
Uses: Food containers, Housewares, Toys
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.952
g/cc
0.0344
lb/in³
ASTM D4883
ESCR 10% Igepal®
<=
2.0
hour
<=
2.0
hour
F-50; Cond. B; ASTM D-1693
Linear Mold Shrinkage
0.016
cm/cm
0.016
in/in
Exxon Method
Melt Flow
19
g/10 min
@Load 2.16 kg,
Temperature 190 °C
19
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow
47.5
cm
18.7
in
Exxon Method
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
24.1
MPa
3500
psi
ASTM D638
Elongation at Yield
19 %
19 %
ASTM D638
Flexural Modulus
0.648
GPa
94.0
ksi
ASTM D790
Thermal Properties
Metric
English
Comments
Melting Point
131
°C
268
°F
Exxon Method
Brittleness Temperature
<=
-70.0
°C
<=
-94.0
°F
ASTM D746
Processing Properties
Metric
English
Comments
Nozzle Temperature
215
°C
419
°F
Nozzle (Melt)
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow DMDA-8920 NT 7 High Density Polyethylene Resin
PEXCA6 / 37825
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.