MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® HD-6733 HDPE, Injection Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Data Provided by Exxon Chemical Canada.

Characteristics: High Flow, Good Stiffness

Uses: Food containers, Small pails, Nursery containers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D4883
ESCR 10% Igepal® <= 2.0 hour<= 2.0 hourF-50; Cond. B; ASTM D-1693
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inExxon Method
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
33 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 55.8 cm22.0 inExxon Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.1 MPa3210 psiASTM D638
Elongation at Yield 20 %20 %ASTM D638
Flexural Modulus 0.558 GPa80.9 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FExxon Method
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 260 °C500 °FNozzle (Melt)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
ExxonMobil HD 50330 High Density Polyethylene Copolymer Resin
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade

PEXCA8 / 37827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.