MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processability

Applications: furniture, small appliances, housewares

Description: Astryn BA65H conventional melt flow, UL 94 V-2 flame tretardant polypropylene copolymer has an excellent cobination of properties and processability. It was designed for application which require flame and heat resistance, along with good electrical properties, high impact strenght and good surface quality.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792B
Linear Mold Shrinkage 0.017 cm/cm0.017 in/inTool, Montell
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 25.0 MPa3630 psiASTM D638
Elongation at Break 45 %45 %ASTM D638
Flexural Modulus, 1% Secant 1100 MPa160000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256A
Gardner Impact 27.0 J19.9 ft-lbASTM D3029
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 8.90e+16 ohm-cm8.90e+16 ohm-cmASTM D257
Dielectric Strength 27.1 kV/mm688 kV/inASTM D149
Arc Resistance 133 sec133 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FASTM D648
UL RTI, Mechanical with Impact 115 °C
@Thickness 3.00 mm
239 °F
@Thickness 0.118 in
ASTM UL94
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
Oxygen Index 28 %28 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Astryn BA66K Polypropylene Copolymer, Flame Retardant
AISI Type A6 Tool Steel
RTP Company RTP 199 X 137777 C Polypropylene (PP) Copolymer - High Flow - High Impact - Flame Retardant - UV Stabilized
Avient Maxxam™ FR PP 402 Polypropylene
LyondellBasell Astryn 65F4-2 Polypropylene Homopolymer, 20% Talc

PMO423 / 53630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.