MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Astryn BA66K Polypropylene Copolymer, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, high limiting oxygen index, non-halogenated, good aesthetics, excellent processability

Applications: batteries, electrical components

Description: Astryn BA66K high melt flow, UL 94 V-2 flame tretardant polypropylene copolymer has an excellent cobination of properties and processability. It is non-halogenated and was designed for applications which have stringent flammability requirements.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792B
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inTool, Montell
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8282ASTM D785
Tensile Strength, Yield 21.0 MPa3050 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Flexural Modulus, 1% Secant 1400 MPa203000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/inASTM D256A
Gardner Impact 3.00 J2.21 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Oxygen Index 38 %38 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant
Overview of materials for Polypropylene, Flame Retardant
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant
Avient Maxxam™ FR PP 402 Polypropylene

PMO426 / 53631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.