MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 6 GFC 30 NC Q1B0C001 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Polyamide 6, reinforced with 30% glass fiber and glass bead, heat stabilized, lubricated, for injection molding. Eplamid 6 GFC 30 offers a good surface finish and dimensional stability which is used in many sectors of industry.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inParallel; ISO 294-4
 0.0090 cm/cm0.0090 in/inNormal; ISO 294-4
Ash 30 %30 %ISO 3451-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 130 MPa18900 psiISO 527-2
Elongation at Break 3.0 %3.0 %ISO 527-2
Tensile Modulus 6.20 GPa899 ksiISO 527-2
Flexural Strength 190 MPa27600 psiISO 178
Flexural Modulus 5.60 GPa812 ksiISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
EN 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epsan Eplamid 6 NC HV A3,6 Polyamide 6
Epsan Eplamid 66 GFI 20 NC Q1C0A801 Polyamide 66
Epsan Eplamid 6 FX2 NC Q1B201 Polyamide 6, Halogen Free
Epsan Eplamid 6 FX0 NC Q1B501 Polyamide 6, Halogen Free
Epsan Eplamid 6 FV2 NC Q1B801 Polyamide 6, Halogenated

PEPSAN021 / 186335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.