MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Stratasys® VEROBLUE Rigid Opaque 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: This multi-purpose material is most widely used for visual models, engineering prototypes, product assemblies and RTV molding patterns. Rigid Opaque materials are good material choices for light functional testing, patterns, prototypes and models. Available in multiple colors, the Vero family shares similar mechanical, thermal and electrical properties. The medium shades of VeroBlue™ and VeroGray™ provide the best detail visualization, without glare or darkness.

Formerly VEROBLUE RGD840.

Information provided by Stratasys

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.18 - 1.19 g/cc0.0426 - 0.0430 lb/in³Polymerized
Water Absorption 1.5 - 2.2 %
@Time 86400 sec
1.5 - 2.2 %
@Time 24.0 hour
D-570-98
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 73 - 7673 - 76
Hardness, Shore D 83 - 8683 - 86
Tensile Strength 50.0 - 60.0 MPa7250 - 8700 psiD-638-03
Elongation at Break 15 - 25 %15 - 25 %D-638-05
Modulus of Elasticity 2.00 - 3.00 GPa290 - 435 ksiD-638-04
Flexural Strength 60.0 - 70.0 MPa8700 - 10200 psiD-790-03
Flexural Modulus 1.90 - 2.50 GPa276 - 363 ksiD-790-04
Izod Impact, Notched 0.200 - 0.300 J/cm0.375 - 0.562 ft-lb/inD-256-06
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °C113 - 122 °FD-648-06
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C113 - 122 °FD-648-07
Glass Transition Temp, Tg 48.0 - 50.0 °C118 - 122 °FDMA, E»

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stratasys® TANGOBLACK FLX973 Polyjet™ Simulated Rubber 3D Printing Polymer
Stratasys® VEROWHITEPLUS Rigid Opaque 3D Printing Polymer
Stratasys® TANGOBLACKPLUS FLX980 Polyjet™ Simulated Rubber 3D Printing Polymer
Proto3000 Objet VeroClear FullCure810
Overview of materials for Polylactic Acid (PLA) Biopolymer

PSTRAS939 / 206352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.