MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Stratasys® TANGOBLACK FLX973 Polyjet™ Simulated Rubber 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: PolyJet technology creates precise prototypes that set the standard for finished-product realism. Their fine resolution makes complex shapes, intricate details and smooth surfaces possible. PolyJet 3D Printing works by jetting layers of liquid photopolymer onto a build tray and instantly curing them with UV light. The fine layers build up to create a precise 3D model or prototype. Models are ready to handle right out of the 3D printer, with no post curing needed.

Information provided by Stratasys

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 - 1.15 g/cc1.14 - 1.15 g/ccPolymerized; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 6260 - 62ASTM D2240
Tensile Strength at Break 1.80 - 2.40 MPa261 - 348 psiASTM D412
Elongation at Break 45 - 55 %45 - 55 %ASTM D412
Tear Strength 2.94 - 4.90 kN/m16.8 - 28.0 pliASTM D624
Compression Set 0.50 - 1.5 %0.50 - 1.5 %ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stratasys® TANGOBLACKPLUS FLX980 Polyjet™ Simulated Rubber 3D Printing Polymer
Stratasys® VEROBLUE Rigid Opaque 3D Printing Polymer
Stratasys® TANGOPLUS FLX930 Polyjet™ Simulated Rubber 3D Printing Polymer
ASTM A588 HSLA Steel Grade D, Thickness < 100 mm (4 in.)
ASTM A588 HSLA Steel Grade C, Thickness < 100 mm (4 in.)

PSTRAT260 / 206357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.