MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo CALIBRE™ 300-10 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: CALIBRE™ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBRE™ 300-10 series products are available in 4 additive packages: CALIBRE™ 300: No mold release or UV Stabilizer. CALIBRE™ 301: Mold release. CALIBRE™ 302: UV stabilizer. CALIBRE™ 303: Mold release and UV stabilizer.

Govt. and Industry Standards:

  • CSA (Canadian Standards Association)
  • Underwriters Laboratory, Inc. (UL)
Applications:
  • Appliance
  • Storage media housings
  • Business equipment
  • Electrical components
  • Lighting
  • Transportation
  • Houseware
  • Recreation
  • Packaging applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/A; ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4; ASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7373ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 71.0 MPa10300 psi50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ASTM D638; ISO 527-2/50
Elongation at Break 150 %150 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638; ISO 527-2/50
Tensile Modulus 2.30 GPa334 ksiISO 527-2/50
 2.41 GPa350 ksi50 mm/min; ASTM D638
Flexural Strength 96.5 MPa14000 psiMethod I (3 point load), 2.0 mm/min; ASTM D790
 97.0 MPa14100 psi2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2.0 mm/min; ISO 178
 2.41 GPa350 ksiMethod I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 9.10 J/cm
@Temperature 23.0 °C
17.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 90.0 kJ/m²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180; ASTM D256A
Charpy Impact, Notched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eA
Dart Drop, Total Energy 87.0 J64.2 ft-lb3.39 m/sec; ASTM D3763
Abrasion 4545[%] Taber; ASTM D1004
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Dielectric Constant  3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor  0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
250 V
@Thickness 0.0787 in
Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test 125 °C257 °FIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 128 °C262 °FUnannealed; ASTM D648
 144 °C291 °FAnnealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FUnannealed; ASTM D648; ISO 75-2/A
 141 °C286 °FAnnealed; ISO 75-2/A
Vicat Softening Point 149 °C300 °FRate A (50°C/h); ASTM D1525; ISO 360/B50
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 26 %26 %ISO 4289-2
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542; ISO 489
Haze 1.0 %1.0 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003
 
Descriptive Properties
Average Extent of Burring3 cmASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers Cadon CG 28 ABS Copolymer
INEOS Styrolution Terluran® HI-10 ABS
Overview of materials for Polycarbonate, Extruded
Covestro Makrolon® 2805 Polycarbonate, Injection Grade
GEHR Plastics PET Polyethylene Terephthalate

PZZDWST005 / 142214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.