MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers Cadon CG 28 ABS Copolymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: High rubber content ABS copolymer with very high toughness and medium flow. Excellent impact and fracture resistance even at very low temperatures.

Property data measured at 23°C and 50% RH.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183-1
Melt Flow 14 g/10 min
@Load 10.0 kg,
Temperature 220 °C
14 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min MVR; ISO 1133
 
Chemical PropertiesMetricEnglishComments
Butadiene Content 27 %27 %Lab-IR
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-1,2
Elongation at Break >= 5.0 %>= 5.0 %50 mm/min; ISO 527-1,2
Tensile Modulus 1.60 GPa232 ksi1mm/min.; ISO 527-1,2
Flexural Modulus 1.72 GPa249 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO)  21.0 kJ/m²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 28.0 kJ/m²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 72.0 kJ/m²
@Temperature -40.0 °C
34.3 ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 93.0 °C199 °FB50, 50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Flammability Test 60
@Thickness 1.00 mm
60
@Thickness 0.0394 in
US-FMVSS , mm/min; ISO 3795
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2,12
 
Optical PropertiesMetricEnglishComments
Yellow Index 31 %31 %E313
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °Finjection molding; ISO 294
Mold Temperature 70.0 °C158 °Finjection molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secinjection molding; ISO 294
 
Descriptive Properties
Residual Monomers (%)0.03lab-GC, 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® F223-D PA6, Conditioned, Low/Medium Viscosity
Envalior Akulon® F223-D PA6, Dry, Low/Medium Viscosity
Envalior Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America)
INEOS Styrolution Terluran® HI-10 ABS
Trinseo CALIBRE™ 300-10 Polycarbonate Resin

PELIX929 / 192523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.