MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Thermx® FG15 NC010 15% Glass Reinforced, Food Grade PCT Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced

Material Notes: Attributes and features include:
  • High-temperature assembly: Withstands SMT reflow soldering
  • High-temperature service: Retains useful strength, toughness with age
  • Chemical resistance: auto fluids, circuit board cleaning agents and more
  • Excellent colorability
  • Hydrolysis resistance: Performs well in USCAR Class 4 tests
  • Dimensional stability: Negligible moisture effect
  • Arc tracking resistance: A valuable asset for 42-volt auto electrical applications

Applications include a wide range of injection molded components for electrical, electronics, automotive, appliance, and other industrial and consumer products. Typical parts include circuit board connectors, automotive connectors (headers), lamp sockets and relays.

Specific Notes for this grade: A 15% glass reinforced high performance polyester resin suitable for repeated-use food-contact US FDA applications

Information provided by DuPont.

Celenese acquired the Thermx product line from DuPont in 2010.

Key Words: Polycyclohexylenedimethylene Terephthalate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 3.20 mm
0.0060 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D785
Tensile Strength at Break 62.0 MPa8990 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 97.0 MPa14100 psiASTM D790
Flexural Modulus 4.00 GPa580 ksiASTM D790
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inASTM D256
 0.320 J/cm
@Temperature -40.0 °C
0.600 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 2.56 J/cm4.80 ft-lb/inASTM D4812
 2.14 J/cm
@Temperature -40.0 °C
4.00 ft-lb/in
@Temperature -40.0 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 259 °C498 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C396 °FASTM D648
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 295 - 310 °C563 - 590 °F300°C Optimum
Mold Temperature 150 - 175 °C302 - 347 °F
Drying Temperature 120 - 150 °C248 - 302 °F
Dry Time 4 - 6 hour4 - 6 hourDehumidified Dryer
Moisture Content <= 0.030 %<= 0.030 %Processing Moisture Content

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
Celanese Thermx® FG30GT NC010 PCT
Celanese Thermx® FG20GT NC010 PCT
Envalior Arnite® TV4 461 (PBT+PET)-GF30
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy

PDUT03 / 33827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.