MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

Hafnium, Hf; Plate
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Tensile and/or hardness values are for plate; other property values are typical of the element. Three entries for pure Hf are in MatWeb.

Characteristics:

  • Contains approximately 250 ppm Dioxide which improves ductility
  • High Neutron absorption
  • Forms a stable, dense, self-healing oxide layer
  • High corrosion resistance
  • Allotropic transformation at 1760°C

Applications:

  • Superalloys
  • Alloying with Aluminium, Copper, Magnesium or Titanium
  • Nuclear systems - control rods

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 13.31 g/cc0.4809 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 178.49178.491995
Atomic Number 7272
Thermal Neutron Cross Section 113 barns/atom113 barns/atom
X-ray Absorption Edge 0.18981 Å0.18981 ÅK
 1.09864 Å1.09864 ÅLI
 1.15311 Å1.15311 ÅLII
 1.2957 Å1.2957 ÅLIII
Electronegativity 1.31.3Pauling
Ionic Radius 0.780 Å0.780 ÅCrystal Ionic Radius for Valence +4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 450 MPa65300 psiLongitudinal
 470 MPa68200 psiTransverse
 235 MPa
@Temperature 315 °C
34100 psi
@Temperature 599 °F
Transverse
 275 MPa
@Temperature 315 °C
39900 psi
@Temperature 599 °F
Longitudinal
Tensile Strength, Yield  125 MPa
@Strain 0.02 %,
Temperature 315 °C
18100 psi
@Strain 0.02 %,
Temperature 599 °F
Longitudinal
 165 MPa
@Strain 0.02 %,
Temperature 315 °C
23900 psi
@Strain 0.02 %,
Temperature 599 °F
Transverse
 195 MPa
@Strain 0.02 %,
Temperature 23.0 °C
28300 psi
@Strain 0.02 %,
Temperature 73.4 °F
Longitudinal
 310 MPa
@Strain 0.02 %,
Temperature 23.0 °C
45000 psi
@Strain 0.02 %,
Temperature 73.4 °F
Transverse
Elongation at Break 25 %25 %Longitudinal or Transverse, 50 mm
 45 %
@Temperature 315 °C
45 %
@Temperature 599 °F
Longitudinal, 50 mm
 48 %
@Temperature 315 °C
48 %
@Temperature 599 °F
Transverse, 50 mm
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000355 ohm-cm0.0000355 ohm-cm
Magnetic Susceptibility 4.2e-74.2e-7cgs/g
Critical Magnetic Field Strength, Oersted 12.712.7
Critical Superconducting Temperature 0.128 K0.128 K
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.90 µm/m-°C
@Temperature 20.0 °C
3.28 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.144 J/g-°C0.0344 BTU/lb-°F
Thermal Conductivity 22.0 W/m-K153 BTU-in/hr-ft²-°F
Melting Point 2207 - 2247 °C4005 - 4077 °F
Boiling Point 3100 °C5610 °F
 
Component Elements PropertiesMetricEnglishComments
Hafnium, Hf 100 %100 %
 
Descriptive Properties
Alpha Phase Crystal Structurehcp< 1760°C
Atomic Weight178.5
Beta Phase Crystal Structurebcc> 1760°C
CAS Number7440-58-6

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hafnium, Hf; Rod
Americium, Am
Silver, Ag
Chromium, Cr; Recrystallized
Copper, Cu; Cold-Worked

AMEHf01 / 44

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.