MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals EL-Lene™ H5814J High Density Polyethylene Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Key Characteristics:
  • Good processability
  • High stiffness
  • High impact strength
  • Balanced properties between shrinkage and warpage
  • Odorless
  • Safe for food contact

Recommended Applications: General purpose injection parts such as utensils, office articles, bottle caps, toy parts

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.958 g/cc0.958 g/ccASTM D1505
Environmental Stress Crack Resistance 2.0 hour
@Temperature 50.0 °C
2.0 hour
@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Linear Mold Shrinkage, Flow 0.016 cm/cm
@Thickness 2.00 mm
0.016 in/in
@Thickness 0.0787 in
TPE Method
Linear Mold Shrinkage, Transverse 0.0177 cm/cm
@Thickness 2.00 mm
0.0177 in/in
@Thickness 0.0787 in
TPE Method
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
14 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength at Break 27.0 MPa3920 psiASTM D638
Tensile Strength, Yield 17.7 MPa2560 psiASTM D638
Elongation at Break 620 %620 %ASTM D638
Flexural Modulus 1.23 GPa178 ksiASTM D790
Izod Impact, Notched >= 0.294 J/cm
@Temperature 23.0 °C
>= 0.551 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 122 °C252 °FASTM D1525
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H6105JU High Density Polyethylene Injection Molding
SCG Chemicals EL-Pro™ P840J Polypropylene Injection Molding
SCG Chemicals EL-Pro™ P740J Polypropylene Injection Molding
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Microtherm Group Aeroguard® SD Filament Reinforced Silica Thermal Insulation Panel, Flexible

PSCGC911 / 120665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.