MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9365D TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion grade; complies with FDA-regulations 21 CFR

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ISO 868
Tensile Strength, Ultimate 58.0 MPa8410 psi200 mm/min; DIN 53504
Elongation at Break 342 %342 %200 mm/min; DIN 53504
50% Modulus 26.0 MPa
@Strain 50 %
26.0 MPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus 30.0 MPa
@Strain 100 %
4350 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 50.0 MPa
@Strain 200 %
7250 psi
@Strain 200 %
200 mm/min; DIN 53504
Flexural Modulus 0.335 GPa48.6 ksi2 mm/min; ISO 178
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °FExtrusion
 230 - 240 °C446 - 464 °FInjection
Mold Temperature 60.0 °C140 °F
Drying Temperature 110 °C230 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 3856D TPU
Covestro Desmopan® 385 Thermoplastic Polyurethane
Covestro Desmopan® 9864DU TPU
Covestro Desmopan® 3378A TPU
Covestro Desmopan® 9365D GMP TPU

PCOVEST0717 / 202500

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.