MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) Altech® NXT PP PP-B A 2035/450 GF35 CP 35% Glass Filled PP Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Polypropylene Heterophasic Copolymer, 35% glass fibers. Chemically coupled, high heat stabilized, high stiffness, high toughness. Applications: automotive, various. Pre drying conditions unnecessary

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Linear Mold Shrinkage  0.0010 - 0.0040 cm/cm
@Time 86400 sec
0.0010 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
 0.0020 - 0.0060 cm/cm
@Time 86400 sec
0.0020 - 0.0060 in/in
@Time 24.0 hour
ISO 294-4
Spiral Flow  30.0 cm
@Thickness 1.00 mm
11.8 in
@Thickness 0.0394 in
 80.0 cm
@Thickness 2.00 mm
31.5 in
@Thickness 0.0787 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 66.0 MPa9570 psiISO 527-1/-2
Elongation at Break 3.7 %3.7 %ISO 527-1/-2
Tensile Modulus 6.40 GPa928 ksiISO 527-1/-2
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 5.50 GPa798 ksiISO 178
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
 5.00 J/cm²
@Temperature -40.0 °C
23.8 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 1.00 J/cm²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 168 °C334 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO 75-1/-2
Vicat Softening Point 105 °C221 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 270 °C392 - 518 °Finjection molding
Mold Temperature 20.0 - 90.0 °C68.0 - 194 °Finjection molding
Drying Temperature 80.0 °C
@Time 7200 - 10800 sec
176 °F
@Time 2.00 - 3.00 hour
for superior surface quality

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) Altech® NXT PP PP-H A 2040/456.01 LE GF40 CP 40% Glass Filled PP Homopolymer
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade
Avient Maxxam™ XN-418.G001-1000 Polypropylene Copolymer (PP Copolymer)

PALBIS9916 / 221012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.