MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PMC Polymer Products Avantra® 8930 Ignition Resistant High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: Used for applications in electronics and appliance industries.

Key Words: IRHIPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Melt Flow 10 g/10 min10 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.5 MPa3700 psi
Elongation at Break 60 %60 %
Flexural Modulus 2.14 GPa310 ksi
Izod Impact, Notched 1.28 J/cm2.40 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °F
Flammability, UL94 V-2V-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PMC Polymer Products Avantra® 8330 Ignition Resistant High Impact Polystyrene
Trinseo Magnum™ 1040 ABS, Very High impact
PMC Polymer Products Avantra® 8530B Ignition Resistant High Impact Polystyrene
Omnia Plastica PSU Polysulphone
Solvay MIRATAINE® CAB-A Surfactant

PPMC994 / 217585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.