MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay MIRATAINE® CAB-A Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Secondary surfactant used as a foam booster, foam stabilizer, thickening agent. MIRATAINE CAB/A functions as well as a mollifying agent for anionic based formulations and is recommended for baby and mild personal care products.

C.T.F.A. /I.N.C.I. Name: COCAMIDOPROPYL BETAINE

CAS: 70851 – 07 – 9

Use level: 1 - 10%

Compatibility: All Surfactant Classes

Available in: Latin America

Applications: Mirataine CAB/A is a glycerine free betaine derived from coconut fatty acids. Used primarily as a secondary surfactant in shampoos, skin cleansers and related high foaming personal care products, MIRATAINE CAB/A serves as a foam booster and foam stabilizer. MIRATAINE CAB/A also functions as a thickening agent and irritation mollifying agent for anionic based formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 34 - 36 %34 - 36 %L250
pH 7.0 - 8.07.0 - 8.0L120
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 4.0<= 4.0L039
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceClear, clean liquid
CompositionActive29-31%, Solids-Sodium Chloride, L401
 Sodium Chloride<5.5%, L400

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omnia Plastica PSU Polysulphone
Trinseo Magnum™ 1040 ABS, Very High impact
PMC Polymer Products Avantra® 8930 Ignition Resistant High Impact Polystyrene

WRHOD284 / 137515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.