MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 12, Glass Bead Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Glass Bead Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.820 - 1.49 g/cc0.0296 - 0.0538 lb/in³Average value: 1.29 g/cc Grade Count:20
Water Absorption 0.0110 - 1.70 %0.0110 - 1.70 %Average value: 0.812 % Grade Count:17
Moisture Absorption at Equilibrium 0.00500 - 0.800 %0.00500 - 0.800 %Average value: 0.515 % Grade Count:7
Water Absorption at Saturation 0.800 - 1.70 %0.800 - 1.70 %Average value: 1.30 % Grade Count:10
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm0.00100 - 0.00900 in/inAverage value: 0.00731 cm/cm Grade Count:13
Linear Mold Shrinkage, Transverse 0.00700 - 0.0100 cm/cm0.00700 - 0.0100 in/inAverage value: 0.00846 cm/cm Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75.0 - 80.075.0 - 80.0Average value: 78.3 Grade Count:5
Tensile Strength, Ultimate 33.0 - 51.0 MPa4790 - 7400 psiAverage value: 46.0 MPa Grade Count:16
Tensile Strength, Yield 37.0 - 50.0 MPa5370 - 7250 psiAverage value: 46.4 MPa Grade Count:8
Elongation at Break 3.00 - 50.0 %3.00 - 50.0 %Average value: 16.7 % Grade Count:17
Elongation at Yield 5.00 - 10.0 %5.00 - 10.0 %Average value: 7.00 % Grade Count:8
Modulus of Elasticity 1.60 - 3.82 GPa232 - 553 ksiAverage value: 2.63 GPa Grade Count:20
Charpy Impact Unnotched 6.00 J/cm² - NB28.6 ft-lb/in² - NBAverage value: 10.3 J/cm² Grade Count:18
 2.94 J/cm² - NB
@Temperature -30.0 - -30.0 °C
14.0 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 7.03 J/cm² Grade Count:16
Charpy Impact, Notched 0.399 - 0.600 J/cm²1.90 - 2.86 ft-lb/in²Average value: 0.456 J/cm² Grade Count:18
 0.294 - 0.600 J/cm²
@Temperature -30.0 - -30.0 °C
1.40 - 2.86 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.365 J/cm² Grade Count:18
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+13 ohm-cm1.00e+9 - 1.00e+13 ohm-cmAverage value: 2.33e+12 ohm-cm Grade Count:12
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 1.11e+14 ohm Grade Count:9
Dielectric Strength 31.0 - 40.0 kV/mm787 - 1020 kV/inAverage value: 37.5 kV/mm Grade Count:12
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:10
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 130 µm/m-°C38.9 - 72.2 µin/in-°FAverage value: 88.4 µm/m-°C Grade Count:12
CTE, linear, Transverse to Flow 70.0 - 90.0 µm/m-°C38.9 - 50.0 µin/in-°FAverage value: 80.8 µm/m-°C Grade Count:11
Melting Point 178 - 185 °C352 - 365 °FAverage value: 178 °C Grade Count:13
Maximum Service Temperature, Air 90.0 - 150 °C194 - 302 °FAverage value: 126 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 180 °C176 - 356 °FAverage value: 147 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 170 °C122 - 338 °FAverage value: 77.2 °C Grade Count:14
Deflection Temperature at 8.0 MPa 40.0 - 145 °C104 - 293 °FAverage value: 84.0 °C Grade Count:10
Flammability, UL94 HBHBGrade Count:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12, 20% Glass Fiber Filled
Overview of materials for Nylon 12
Overview of materials for Nylon 12, Carbon Fiber Filled
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
Overview of materials for Nylon 12, 40% Glass Fiber Filled

O2650 / 78072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.