MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek Yttria Partially Stabilized Zirconia, YTZP, Sintered
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.

Data Provided by the manufacturer, Coors Ceramics Co.

Key Words: Zirconium Oxide, YSZ
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.02 g/cc0.217 lb/in³ASTM C20
Water Absorption 0.00 %0.00 %ASTM C373
Particle Size 1.0 µm1.0 µmAverage Crystal Size - Thin Section Test
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 12.712.71000 g load
Hardness, Rockwell 45 N 8181GPa
Modulus of Elasticity 210 GPa30500 ksiASTM C848
Flexural Strength 1240 MPa180000 psiASTM F417
Compressive Strength 2500 MPa363000 psiASTM C773
Poissons Ratio 0.230.23ASTM C848
Fracture Toughness 13.0 MPa-m½11.8 ksi-in½Notched Beam
Shear Modulus 85.0 GPa12300 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmASTM D1829
 <= 1000 ohm-cm
@Temperature 1000 °C
<= 1000 ohm-cm
@Temperature 1830 °F
ASTM D1829
 20000 ohm-cm
@Temperature 500 °C
20000 ohm-cm
@Temperature 932 °F
ASTM D1829
Dielectric Constant 29
@Frequency 1e+6 Hz
29
@Frequency 1e+6 Hz
Dielectric Strength 9.00 kV/mm229 kV/inac; ASTM D116
Dielectric Loss Index 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D2520
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.3 µm/m-°C
@Temperature 25.0 - 1000 °C
5.72 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°FASTM E1269
Thermal Conductivity 2.20 W/m-K15.3 BTU-in/hr-ft²-°FASTM C408
Maximum Service Temperature, Air 1500 °C2730 °FNo Load
 
Descriptive Properties
ColorIvory

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoorsTek ZDY Yttria Fully Stabilized Zirconia
Alumina, alpha Al2O3, 99.5%
Aluminum Nitride, AlN
CoorsTek PlasmaPure™ AD-998 Alumina (nom. 99.8% Al2O3)
CoorsTek PlasmaPure-UC™ 99.9% Alumina

CZ3C / 2743

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.