MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Primef® 7010 Polyphenylene Sulfide (PPS), 65% Glass\Mineral  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less fluidity. In general, PPS offers an excellent balance of properties including high temperature resistance, chemical resistance, dimensional stability and electrical characteristics. Because of its inherent flame retardancy, PPS is a good choice for high-temperature electrical and electronic applications.

Features: Flame Retardant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Strength; High Flow; High Heat Resistance; Low to No Water Absorption

Uses:

Availability: Europe

Holding Time: 3 sec
Cooling Time, 2 mm: 2.5 sec

Information provide by Solvay Specialty Polymers

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.96 g/cc0.0708 lb/in³ISO 1183
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa
@Temperature 23.0 °C
23200 psi
@Temperature 73.4 °F
ISO 527-2
Elongation at Break 1.2 %
@Temperature 23.0 °C
1.2 %
@Temperature 73.4 °F
ISO 527-2
Tensile Modulus 21.0 GPa
@Temperature 23.0 °C
3050 ksi
@Temperature 73.4 °F
ISO 527-2
Flexural Strength 240 MPa
@Temperature 23.0 °C
34800 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 21.0 GPa
@Temperature 23.0 °C
3050 ksi
@Temperature 73.4 °F
ISO 178
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256
Izod Impact, Unnotched 2.80 J/cm5.25 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant  4.9
@Frequency 1e+6 Hz
4.9
@Frequency 1e+6 Hz
IEC 60250
 5.0
@Frequency 1000 Hz
5.0
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm381 kV/inIEC 60243-1
Dissipation Factor  0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
 0.030
@Frequency 1000 Hz
0.030
@Frequency 1000 Hz
IEC 60250
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.600 W/m-K4.16 BTU-in/hr-ft²-°FISO 8302
Maximum Service Temperature, Air 220 °C428 °FASTM D794
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Oxygen Index 58 %58 %ISO 4598-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 290 - 300 °C554 - 572 °F
Middle Barrel Temperature 310 - 320 °C590 - 608 °F
Front Barrel Temperature 320 - 330 °C608 - 626 °F
Nozzle Temperature 320 - 350 °C608 - 662 °F
Melt Temperature 320 - 330 °C608 - 626 °F
Mold Temperature 150 - 160 °C302 - 320 °F
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 30.0 - 150 MPa4350 - 21800 psi
Back Pressure 0.000 - 1.00 MPa0.000 - 145 psi
Screw Speed 3.0 - 10 rpm3.0 - 10 rpm
 
Descriptive Properties
Additional PropertiesSpiral Flow Length - Internal Method: 90.0 mm
FormsPellets
Injection RateFast
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, Conditioned
Syensqo (Solvay Specialty Polymers) Primef® 7002 Polyphenylene Sulfide (PPS), 65% Glass\Mineral
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Celanese Celanex® 2300 GV1/20 PBT, 20% Glass Reinforced

PSOLVAY178 / 122476

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.