MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 92 E 4670 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction IROGRAN A 92 E 4670 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a specially designed, flexible material with a broad processing window.

Performance Features:

  • High oil resistance
  • High production rate
  • Good melt flow
  • Easy coloring
  • Complies with FDA CFR 175.105 /177.2600
Applications:
  • Cable jacketing
  • Tubing
  • Technical extrusion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Injection molded parts; ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inInjection molded; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090Injection molded parts; ASTM D2240
Hardness, Shore D 3838Injection molded parts; ASTM D2240
Tensile Strength at Break 36.0 MPa5220 psiInjection molded parts; DIN 53504
Elongation at Break 600 %600 %Injection molded parts; DIN 53504
100% Modulus 8.50 MPa
@Strain 100 %
1230 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 16.0 MPa
@Strain 300 %
2320 psi
@Strain 300 %
Injection molded parts; DIN 53504
Rebound 1.21 %1.21 %Bayshore
Tear Strength 80.6 kN/m460 pliInjection molded parts; ASTM D624
Abrasion 2020mm3, Injection molded; DIN 53516
Compression Set  25 %
@Temperature 22.8 °C,
Time 86400 sec
25 %
@Temperature 73.0 °F,
Time 24.0 hour
Injection molded; ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 - 170 °C257 - 338 °F0.025" extruded film,
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester
Teknor Apex Laripur® LPR 9060EF Thermoplastic Polyurethane
Austin Novel Materials Texalan® 298A Polyester-based TPU
Covestro DUREFLEX® U073 TPU
Covestro DUREFLEX® PT1710S TPU

PHUQ100 / 159473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.