MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PSC 1441 Easy Flow, High Heat Resistance Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Total Petrochemicals Polystyrene 1441 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact polystyrene. Having high gloss, it is particularly suitable for glossy-layer co-extrusion.

In injection molding, 1441, possesses low viscosity at high shear rate. It does combine excellent fluidity with a higher softening point.

Suitable applications for Total Petrochemicals Polystyrene 1441 include dairy sheet, cups (dilution with HIPS), boxes, office equipment - e.g. filing trays, CD boxes, pen bodies and internal fridge parts.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Water Absorption 0.040 %0.040 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 7070ASTM D785
Tensile Strength at Break 48.0 MPa6960 psiASTM D638
Tensile Strength, Yield 48.0 MPa6960 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Modulus 3.10 GPa450 ksiASTM D790
Izod Impact, Notched (ISO) 1.50 kJ/m²0.714 ft-lb/in²ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmISO IEC 93
Dielectric Strength 152 kV/mm3860 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 89.0 µm/m-°C49.4 µin/in-°FASTM D696
Vicat Softening Point 98.0 °C
@Load 1.02 kg
208 °F
@Load 2.25 lb
50°C per hour; ASTM D1525
Heat Distortion Temperature 83.9 °C183 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSC 1540(AS) Crystal Polystyrene
Total PSC 1540(EU) Crystal Polystyrene
Total PSC 1340 Crystal Polystyrene
Total PSC 1160/1160N Crystal Polystyrene
KKPC Kuhmo GP 100 High Flow GPPS

PTOTAL882 / 130607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.