MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit 2920 W Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: Mineral and organic filled molding compound with good dimensional stability and heat resistance.

USES: Carburettor and intake manifold thermal insulator.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 - 0.850 g/cc0.0271 - 0.0307 lb/in³Powder Density; ISO 60
Density 1.75 g/cc0.0632 lb/in³Relative Density; ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inInjection Molding; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 - 50.0 MPa5800 - 7250 psiISO 527
Elongation at Break 0.65 - 0.75 %0.65 - 0.75 %Tensile; ISO 527
Tensile Modulus 10.5 - 12.0 GPa1520 - 1740 ksiISO 527
Flexural Strength 80.0 - 100 MPa11600 - 14500 psiAt Rupture; ISO 178
Flexural Modulus 6.00 - 8.00 GPa870 - 1160 ksiISO 178
Flexural Strain at Break 1.2 - 1.3 %1.2 - 1.3 %ISO 178
Compressive Strength 200 - 230 MPa29000 - 33400 psiISO 604
Charpy Impact Unnotched 0.650 - 0.800 J/cm²3.09 - 3.81 ft-lb/in²ISO 179
Charpy Impact, Notched 0.200 - 0.300 J/cm²0.952 - 1.43 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+10 - 1.00e+11 ohm1.00e+10 - 1.00e+11 ohmDry; IEC 167
Dielectric Strength 25.0 kV/mm635 kV/inIEC 243
Comparative Tracking Index 175 V175 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 - 40.0 µm/m-°C
@Temperature 20.0 °C
16.7 - 22.2 µin/in-°F
@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C
@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F
@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 150 - 180 °C302 - 356 °FISO 75 Af
Deflection Temperature at 8.0 MPa 130 - 150 °C266 - 302 °FISO 75 C
Flammability, UL94  V-1
@Thickness 1.60 mm
V-1
@Thickness 0.0630 in
 V-0
@Thickness 4.00 mm
V-0
@Thickness 0.157 in
Shrinkage 0.10 - 0.20 %0.10 - 0.20 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
ISO typePF 2 C3
Main FillerMineral & Organic
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit X658 Novolac Phenolic
Vyncolit 3640 CG Novolac Phenolic
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound
Sumitomo Bakelite North America RX® 865M Novolac Phenolic
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate

PVYNC034 / 72242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.