MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® FC 182 PTFE, Bronze powder/ Molybdenum Disulfide Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Description: Fluon® FC 182 (310 182 141) is a bronze powder / molybdenum disulfide filled PTFE product. This compound is supplied dry powder form.

End Uses: Bronze powder & molybdenum disulfide are added to PTFE to increase the thermal and electrical conductivity and to improve the wear properties and deformation resistance without sacrificing the chemical and thermal resistance of the polymer.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.64 g/cc3.64 g/ccASTM D4745
Filler Content 60 %60 %ASTM D4745
Deformation 1.8 %1.8 %under load
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464Sustained; ASTM D2240
 6666Peak; ASTM D2240
Tensile Strength 15.9 MPa2300 psiASTM D4745
Elongation at Break 130 %130 %ASTM D4745
Coefficient of Friction, Dynamic 0.130.13ASTM D3702
K (wear) Factor 10.1 x 10-8 mm³/N-M5.00 x 10-10 in³-min/ft-lb-hr5000 PV; ASTM D3702

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC FC 482 PTFE, 55% Bronze/ 5% Moly
AGC Fluon® RA3540 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound
AGC Fluon® PA7115 15% Polyimide, PTFE Filled Compound
AGC Fluon® FC 435 PTFE, 25% Carbon Filled
AGC Fluon® FC 433 PTFE, 15% Carbon Filled

PAGCX091 / 191200

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.