MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen CRP 100 S RED High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Hostalen CRP 100 S red is a high density polyethylene (HDPE), red colored similar RAL 3020 with light stabilizer and high melt viscosity for identification marking stripes for electrical cable protection pipes made from Hostalen CRP 100 black.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183-1
Oxidative Induction Time (OIT) >= 20 min
@Temperature 210 °C
>= 20 min
@Temperature 410 °F
ISO 11357-6
Melt Flow 0.45 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.45 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 
Descriptive Properties
Processing Methodsheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
LyondellBasell Hostalen CRP 100 BLACK (XL) High Density Polyethylene (HDPE), Pipe Grade
NOVA Chemicals NOVAPOL® HE-Y449-AC HDPE Pipe Extrusion Resin
Total XLS 12 B High Density Polyethylene - Pipes and Fittings

PEQT8474 / 220109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.