MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Momentive Performance Materials TSE3261-G Heat Resistant Silicone Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: TSE3261-G is a one-component heat curable silicone adhesive designed for high temperature applications. TSE3261-G adheres well to a variety of substrates such as metals, plastics, ceramics and glass without the use of a primer.

Cured properties for specimen cured 1 hour at 150°C.

Key Performance Properties:

  • Ready to use - one component
  • Excellent high temperature resistance
  • Heat accelerated cure
  • Excellent adhesive properties; primerless adhesion to many types of substrates
  • Gray color
  • Non corrosive to metals

Applications:

  • Sealing and bonding for high temperature applications
    • Heaters
    • Steam Irons
    • Microwave Ovens
  • Sealing, bonding and potting for electrical appliances and electronic parts.

    GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc
@Temperature 23.0 °C
1.48 g/cc
@Temperature 73.4 °F
Viscosity 80000 cP80000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5454
Tensile Strength at Break 4.90 MPa711 psi
Elongation at Break 160 %160 %
Adhesive Bond Strength 1.77 MPa257 psiAluminum lap shear
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cm
Dielectric Constant 3.33.3
Dielectric Strength 22.0 kV/mm559 kV/in
Dissipation Factor 0.0200.020
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorGray
ConsistencyFlowable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE3281G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive
Momentive Performance Materials SLA7401-D1 Silicone Laminating Adhesive, Thermal Cure

PGESIL068 / 41059

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.