MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: TSE 3221 is a one-component, flowable, heat curing adhesive which is translucent in color and offers primerless adhesion to a wide variety of substrates. This product requires an elevated temperature cure and exhibits very low linear shrinkage.

Key Performance Properties:

  • One component product-no mixing required
  • Fast cure at elevated temperature
  • Primerless adhesion to many types of substrates
  • No cure by-products, low linear shrinkage
  • Non-corrosive to metals and sensitive substrates
  • Excellent dielectric properties
  • Outstanding performance over a wide thermal range

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/cc
Viscosity 55000 cP55000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2828
Tensile Strength, Ultimate 2.35 MPa341 psi
Elongation at Break 290 %290 %
Adhesive Bond Strength 1.96 MPa284 psiAluminum to aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cm
Dielectric Constant 2.82.8
Dielectric Strength 21.02 kV/mm533.9 kV/in
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 90.0 min
@Temperature 125 °C
1.50 hour
@Temperature 257 °F
 180 min
@Temperature 100 °C
3.00 hour
@Temperature 212 °F
 
Descriptive Properties
ColorTranslucent
ConsistencyFlowable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE3261-G Heat Resistant Silicone Adhesive
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
Momentive Performance Materials TSE3281G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials SLA7401-D1 Silicone Laminating Adhesive, Thermal Cure

PGESIL066 / 41057

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.