MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant

Processing Method: Injection Molding

Forms: Pellets

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm0.0090 - 0.014 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength 72.4 MPa10500 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 3.21 GPa465 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 16.9 kV/mm
@Thickness 3.00 mm
430 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 600 V600 VUL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 257 °C495 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 224 °C435 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FUnannealed; ASTM D648
UL RTI, Electrical  120 °C
@Thickness 0.810 mm
248 °F
@Thickness 0.0319 in
UL 746
 120 °C
@Thickness 1.50 mm
248 °F
@Thickness 0.0590 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  95.0 °C
@Thickness 0.810 mm
203 °F
@Thickness 0.0319 in
UL 746
 105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0590 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  120 °C
@Thickness 0.810 mm
248 °F
@Thickness 0.0319 in
UL 746
 120 °C
@Thickness 1.50 mm
248 °F
@Thickness 0.0590 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
Flammability, UL94 V-0
@Thickness 0.569 mm
V-0
@Thickness 0.0224 in
Oxygen Index 33 %33 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 246 - 257 °C475 - 495 °F
Middle Barrel Temperature 263 - 268 °C505 - 515 °F
Front Barrel Temperature 263 - 274 °C505 - 525 °F
Nozzle Temperature 268 - 279 °C515 - 535 °F
Melt Temperature 263 - 277 °C505 - 530 °FProcessing Temperature
Drying Temperature 79.4 °C175 °F
Moisture Content 0.20 %0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Domo TECHNYL® B 50 H1 PA66/6, DRY
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, DRY
Syensqo (Solvay Specialty Polymers) Primef® 7010 Polyphenylene Sulfide (PPS), 65% Glass\Mineral

PTEKNO443 / 128620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.