MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A34 01 PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 8.5 %8.5 %ISO 62
Moisture Absorption at Equilibrium 2.2 %2.2 %23°C/50% R.H.; ISO 62
Relative Viscosity 3.5 cP3.5 cPISO Test; 96 % SAV
Viscosity Number 205 cm³/g2.05 dl/g
Linear Mold Shrinkage 0.014 cm/cm0.014 in/inASTM Data; MD
Melt Flow 40 g/10 min
@Load 5.00 kg,
Temperature 275 °C
40 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psi50mm/min; ISO 527
 80.0 MPa11600 psi2 in/min; ASTM Test
Elongation at Break 25 %25 %50mm/min, Nominal strain; ISO 527
 50 %50 %2 in/min; ASTM Test
Elongation at Yield 4.2 %4.2 %50mm/min; ISO 527
Tensile Modulus 3.20 GPa464 ksi1mm/min; ISO 527
 3.20 GPa464 ksiASTM Test
Flexural Modulus 2.76 GPa400 ksiASTM Test
Izod Impact, Notched 0.530 J/cm
@Temperature -40.0 °C
0.993 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 0.640 J/cm
@Thickness 3.17 mm
1.20 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 60250
 0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
CTE, linear, Parallel to Flow 85.0 µm/m-°C47.2 µin/in-°FISO 11359
Melting Point 255 °C491 °F10 K/min
 260 °C500 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 199 °C390 °FASTM Test
 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75
 100 °C212 °FASTM Test
Vicat Softening Point 250 °C482 °F(50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94  V-2
@Thickness 1.57 mm
V-2
@Thickness 0.0618 in
 V-2
@Thickness 0.890 mm
V-2
@Thickness 0.0350 in
Oxygen Index 28 %28 %ISO 4589-1/-2
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueFilm Extrusion
ProcessingInjection Molding
 Other Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A34 01 PA66 (Conditioned)
BASF Ultramid® 8202 PA6 (Conditioned)
BASF Ultramid® A27 E 01 PA66 (Dry)
GEHR Plastics PA 6.6 Nylon 6.6, Dry
BASF Ultramid® A27 E 01 PA66 (Conditioned)

PBASF9215 / 84979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.