MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in combination with a balance of strength, stiffness and excellent moldability/surface aesthetics.

Applications: front wheel chair wheels, bicycle wheels, power tool housings, chain saw housings, clips and fasteners, hose clamps and window hardware.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.90 %0.90 %24 hour; ASTM D570
 1.5 %1.5 %50% RH; ASTM D570
 5.5 %5.5 %Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm0.00762 in/in1/8" bar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121
Tensile Strength at Break 145 MPa21000 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 232 MPa33600 psiISO 790
Flexural Modulus 7.99 GPa1160 ksiISO 178
Izod Impact, Notched (ISO) 182 kJ/m²86.6 ft-lb/in²ISO 3146
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 208 °C406 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 1 245 - 275 °C473 - 527 °FRear Zone
Zone 2 260 - 285 °C500 - 545 °FCenter Zone
Zone 3 270 - 295 °C518 - 563 °FFront Zone
Zone 4 270 - 295 °C518 - 563 °FNozzle
Melt Temperature 270 - 295 °C518 - 563 °F
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.080 %<= 0.080 %
 
Descriptive Properties
ColorBK 106
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry)
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)

PBASG0419 / 132052

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.