Amphora™ Flex 3D polymer FL6000, a flexible material engineered for extrusion-based additive manufacturing processes. Amphora Flex FL6000 is a polymer that can be used with standard 3D printers, eliminating the need to switch to specialized flex extruders. Because of exceptional layer-to-layer adhesion and melt strength, it prints at a faster speed than other elastomeric materials, saving time. Amphora Flex FL6000 is an engineering-grade material that demonstrates superior durability and toughness, enabling designers to quickly create truly functional parts that can withstand the rigors of everyday use. Amphora Flex FL6000 is highly useful for applications that demand both the durability of an engineering-grade polymer and the comfort and utility of a flexible material. With a Shore A hardness level of 95, outstanding chemical resistance, and a temperature resistance that allows steam sterilization, users may find it useful for additive manufacturing of prosthetics, orthotics, automotive parts, apparel, tooling, or a variety of consumer products. Application/Uses: - Production of 3D Printing filaments
Key Attributes:- Dimensional stability
- Enhanced aesthetics
- Excellent Temperature Resistance
- Excellent toughness
- Extended Processing Window
- Low odor
- Property retention in 3D applications
- Steam Sterilizable
- Styrene-free
- Workability
|
 Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |