MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax SB786 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: blush-resistant, easy molding, high impact polypropylene copolymer resin, good cold impact resistance, good stiffness, FDA acceptable

Applications: automotive battery case, housewares, closures

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax SB786 easy molding, blush-resistant, high impact polypropylene copolymer resin is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. It has a UL yellow card RTI, which applies to all colors.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792B
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Yield 8.0 %8.0 %ASTM D638
Flexural Modulus, 1% Secant 1200 MPa174000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256A
Impact Test 29.0 J
@Temperature -29.0 °C
21.4 ft-lb
@Temperature -20.2 °F
Montell drop weight impact strength
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C189 °FASTM D648
UL RTI, Mechanical with Impact 115 °C
@Thickness >=0.940 mm
239 °F
@Thickness >=0.0370 in
Flammability, UL94 HB
@Thickness >=0.940 mm
HB
@Thickness >=0.0370 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
IRPC Polimaxx Polene 1100NK Polypropylene Homopolymer
LyondellBasell Montell SE191 Polypropylene Impact Copolymer
LyondellBasell Pro-fax 7523 Polypropylene Impact Copolymer

PMO204 / 53557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.