MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Commercially Pure Titanium.

Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3, 4, 5.

Features: The mechanical properties of CP titanium are influenced by small additions of oxygen and iron. By careful control of these additions, the various grades of commercially pure titanium are produced to give properties suited to different applications. TIMETAL 50A is equivalent to ASTM Grade 2. It is the "workhorse" for industrial applications, having a guaranteed minimum 0.2% yield strength and good ductility and formability. It is used extensively for sea water piping, reactor vessels and heat exchangers throughout the CPI, Petrochemical, Oil and Gas and Naval/Marine markets. This alloy is also ASME approved, has good impact properties at low temperatures, and has excellent resistance to erosion and corrosion by seawater and marine atmospheres. It can be easily welded, machined, cold worked, hot worked, and cast. It is nonmagnetic.

Typical heat treatment for this alloy: Anneal at 700°C for 1 hour and air cool. Stress Relieve at 500°C for 30 mins and air cool.

Data provided by TIMET.

Key Words: UNS R50400
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.51 g/cc0.163 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 485 MPa70300 psiTypical
 178 MPa
@Temperature 450 °C
25800 psi
@Temperature 842 °F
 186 MPa
@Temperature 400 °C
27000 psi
@Temperature 752 °F
 229 MPa
@Temperature 300 °C
33200 psi
@Temperature 572 °F
 280 MPa
@Temperature 200 °C
40600 psi
@Temperature 392 °F
 383 MPa
@Temperature 100 °C
55500 psi
@Temperature 212 °F
Tensile Strength, Yield 345 MPa
@Strain 0.2 %
50000 psi
@Strain 0.2 %
Typical
 74.0 MPa
@Strain 0.2 %,
Temperature 450 °C
10700 psi
@Strain 0.2 %,
Temperature 842 °F
 92.0 MPa
@Strain 0.2 %,
Temperature 400 °C
13300 psi
@Strain 0.2 %,
Temperature 752 °F
 127 MPa
@Strain 0.2 %,
Temperature 300 °C
18400 psi
@Strain 0.2 %,
Temperature 572 °F
 192 MPa
@Strain 0.2 %,
Temperature 200 °C
27800 psi
@Strain 0.2 %,
Temperature 392 °F
 256 MPa
@Strain 0.2 %,
Temperature 100 °C
37100 psi
@Strain 0.2 %,
Temperature 212 °F
Elongation at Break 28 %28 %Typical
 31 %
@Temperature 100 °C
31 %
@Temperature 212 °F
 34 %
@Temperature 450 °C
34 %
@Temperature 842 °F
 37 %
@Temperature 200 °C
37 %
@Temperature 392 °F
 38 %
@Temperature 400 °C
38 %
@Temperature 752 °F
 43 %
@Temperature 300 °C
43 %
@Temperature 572 °F
Reduction of Area 57 %57 %Typical
Modulus of Elasticity 105 - 120 GPa15200 - 17400 ksiTypical
Fatigue Strength  154 MPa
@# of Cycles 1.00e+7
22300 psi
@# of Cycles 1.00e+7
Notched, Kt=3; rotating bend
 232 MPa
@# of Cycles 1.00e+7
33600 psi
@# of Cycles 1.00e+7
Smooth, Kt=1; rotating bend
Bend Radius, Minimum 2.5 t2.5 tTypical; on 0.078 in (2 mm) sheet
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000530 ohm-cm0.0000530 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.60 µm/m-°C
@Temperature 20.0 - 100 °C
4.78 µin/in-°F
@Temperature 68.0 - 212 °F
 9.50 µm/m-°C
@Temperature 20.0 - 300 °C
5.28 µin/in-°F
@Temperature 68.0 - 572 °F
 9.70 µm/m-°C
@Temperature 20.0 - 500 °C
5.39 µin/in-°F
@Temperature 68.0 - 932 °F
Thermal Conductivity 21.79 W/m-K151.2 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 425 °C797 °FContinuous
 540 °C1000 °FIntermittent
Beta Transus 915 °C1680 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.030 %<= 0.030 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.25 %<= 0.25 %
Titanium, Ti >= 98.9 %>= 98.9 %Calculated as remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2
Titanium Grade 2, Annealed
Titanium Ti-6Al-4V (Grade 5), Annealed
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1)
Titanium Grade 1

NTIME50A / 19301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.