MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Commercially Pure Titanium.

Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.

Features: The mechanical properties of CP titanium are influenced by small additions of oxygen and iron. By careful control of these additions, the various grades of commercially pure titanium are produced to give properties suited to different applications. TIMETAL 35A contains the lowest oxygen and iron levels, producing the most formable grade of material. It has the highest purity, lowest strength, and best room-temperature ductility and formability of the four ASTM commercially pure grades. 35A should be used where maximum formability is required such as in explosive bonding and plate type heat exchangers. It exhibits excellent corrosion resistance in highly oxidizing to mildly reducing environments, including chlorides. It has good impact properties at low temperatures. In addition, TIMETAL 35A can be easily welded, machined, cold worked, hot worked, and cast. It is nonmagnetic.

Typical heat treatment for this alloy: Anneal at 700°C for 1 hour and air cool. Stress Relieve at 500°C for 30 mins and air cool.

Data provided by TIMET.

Key Words: UNS R50250
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.51 g/cc0.163 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 345 MPa50000 psiTypical
 114 MPa
@Temperature 450 °C
16500 psi
@Temperature 842 °F
 130 MPa
@Temperature 400 °C
18900 psi
@Temperature 752 °F
 163 MPa
@Temperature 300 °C
23600 psi
@Temperature 572 °F
 219 MPa
@Temperature 200 °C
31800 psi
@Temperature 392 °F
 284 MPa
@Temperature 100 °C
41200 psi
@Temperature 212 °F
Tensile Strength, Yield 220 MPa
@Strain 0.2 %
31900 psi
@Strain 0.2 %
Typical
 31.0 MPa
@Strain 0.2 %,
Temperature 450 °C
4500 psi
@Strain 0.2 %,
Temperature 842 °F
 36.0 MPa
@Strain 0.2 %,
Temperature 400 °C
5220 psi
@Strain 0.2 %,
Temperature 752 °F
 51.0 MPa
@Strain 0.2 %,
Temperature 300 °C
7400 psi
@Strain 0.2 %,
Temperature 572 °F
 85.0 MPa
@Strain 0.2 %,
Temperature 200 °C
12300 psi
@Strain 0.2 %,
Temperature 392 °F
 156 MPa
@Strain 0.2 %,
Temperature 100 °C
22600 psi
@Strain 0.2 %,
Temperature 212 °F
Elongation at Break 35 %35 %Typical
 38 %
@Temperature 100 °C
38 %
@Temperature 212 °F
 40 %
@Temperature 200 °C
40 %
@Temperature 392 °F
 48 %
@Temperature 300 °C
48 %
@Temperature 572 °F
 49 %
@Temperature 450 °C
49 %
@Temperature 842 °F
 51 %
@Temperature 400 °C
51 %
@Temperature 752 °F
Reduction of Area 70 %70 %Typical
Modulus of Elasticity 105 - 120 GPa15200 - 17400 ksiTypical
Fatigue Strength  123 MPa
@# of Cycles 1.00e+7
17800 psi
@# of Cycles 1.00e+7
Notched, Kt=3; rotating bend
 193 MPa
@# of Cycles 1.00e+7
28000 psi
@# of Cycles 1.00e+7
Smooth, Kt=1; rotating bend
Bend Radius, Minimum 2.0 t
@Thickness 2.00 mm
2.0 t
@Thickness 0.0787 in
Typical; sheet
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000450 ohm-cm0.0000450 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.60 µm/m-°C
@Temperature 20.0 - 100 °C
4.78 µin/in-°F
@Temperature 68.0 - 212 °F
 9.50 µm/m-°C
@Temperature 20.0 - 300 °C
5.28 µin/in-°F
@Temperature 68.0 - 572 °F
 9.70 µm/m-°C
@Temperature 20.0 - 500 °C
5.39 µin/in-°F
@Temperature 68.0 - 932 °F
Thermal Conductivity 21.97 W/m-K152.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 425 °C797 °FContinuous
 540 °C1000 °FIntermittent
Beta Transus 890 °C1630 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.030 %<= 0.030 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.18 %<= 0.18 %
Titanium, Ti >= 99.1 %>= 99.1 %Calculated as remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2, Annealed
Titanium Grade 2
Titanium Grade 1, Annealed
Titanium Grade 1
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2)

NTIME35A / 19299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.