MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Ovation Polymers Nemcon™ H ABS DP116P ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.

Information provided by Ovation Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.66 g/cc1.66 g/ccASTM D792
Maximum Moisture Content 0.0200.020%
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 32.0 MPa4640 psi50 mm/min; ASTM D638
Elongation at Break 1.7 %1.7 %50 mm/min; ASTM D638
Tensile Modulus 3.572 GPa518.1 ksi50 mm/min; ASTM D638
Flexural Strength 52.0 MPa7540 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.188 GPa462.4 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.214 J/cm
@Temperature 23.0 °C
0.401 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 8.00e+12 ohm8.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°FASTM E-1461
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
@Thickness 3.20 mm
178 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 270 °C428 - 518 °F
Zone 1 220 - 255 °C428 - 491 °F
Zone 2 220 - 260 °C428 - 500 °F
Zone 3 220 - 265 °C428 - 509 °F
Melt Temperature 220 - 275 °C428 - 527 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 70.0 - 90.0 °C158 - 194 °F
Dry Time 4 - 6 hour4 - 6 hour
Back Pressure 0.207 - 0.552 MPa30.0 - 80.0 psi
Screw Speed 70 - 100 rpm70 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovation Polymers Nemcon™ E ABS 20CF
Ovation Polymers SOFTAPLAS™ S 75A Thermoplastic Elastomer
Ovation Polymers Nemcon™ E HDPE 11000
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate
Ovation Polymers Nemcon™ E PET 30131 PET

POVAT124 / 55837

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.