MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep deformation resistance.

Applications:Heat treatment industry-conveyor belts, rollers, burner parts, refractory supports, retorts linings, oven linings, fans, tube hangers, baskets, and trays. Chemical process industry- containers for hot concentrated acids, ammonia, and sulfur dioxide. Food processing industry- used in contact with hot acetic and citric acid.

Typical property data reported.

Key Words: UNS S31000
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.03 g/cc0.290 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 617 MPa89500 psiASTM E8
 48.0 MPa
@Temperature 1093 °C
6960 psi
@Temperature 1999 °F
ASTM E8
 76.0 MPa
@Temperature 871 °C
11000 psi
@Temperature 1600 °F
ASTM E8
 209 MPa
@Temperature 816 °C
30300 psi
@Temperature 1500 °F
ASTM E8
 394 MPa
@Temperature 649 °C
57100 psi
@Temperature 1200 °F
ASTM E8
 483 MPa
@Temperature 538 °C
70100 psi
@Temperature 1000 °F
ASTM E8
 516 MPa
@Temperature 427 °C
74800 psi
@Temperature 801 °F
ASTM E8
 528 MPa
@Temperature 204 °C
76600 psi
@Temperature 399 °F
ASTM E8
Tensile Strength, Yield  136 MPa
@Temperature 816 °C
19700 psi
@Temperature 1500 °F
ASTM E8
 156 MPa
@Temperature 649 °C
22600 psi
@Temperature 1200 °F
ASTM E8
 167 MPa
@Temperature 538 °C
24200 psi
@Temperature 1000 °F
ASTM E8
 188 MPa
@Temperature 427 °C
27300 psi
@Temperature 801 °F
ASTM E8
 217 MPa
@Temperature 204 °C
31500 psi
@Temperature 399 °F
ASTM E8
 292 MPa
@Strain 0.2 %
42400 psi
@Strain 0.2 %
ASTM E8
Elongation at Break 45 %45 %ASTM E8
 36 %
@Temperature 538 °C
36 %
@Temperature 1000 °F
ASTM E8
 37 %
@Temperature 427 °C
37 %
@Temperature 801 °F
ASTM E8
 37.5 %
@Temperature 204 °C
37.5 %
@Temperature 399 °F
ASTM E8
 41.5 %
@Temperature 649 °C
41.5 %
@Temperature 1200 °F
ASTM E8
 65 %
@Temperature 871 °C
65 %
@Temperature 1600 °F
ASTM E8
 66 %
@Temperature 816 °C
66 %
@Temperature 1500 °F
ASTM E8
 77 %
@Temperature 1093 °C
77 %
@Temperature 1999 °F
ASTM E8
Creep Strength  20.0 MPa
@Temperature 788 °C,
Time 3.60e+7 sec
2900 psi
@Temperature 1450 °F,
Time 10000 hour
1% creep
 138 MPa
@Temperature 593 °C,
Time 3.60e+7 sec
20000 psi
@Temperature 1100 °F,
Time 10000 hour
1% creep
Rupture Strength  20.0 MPa
@Temperature 899 °C,
Time 3.60e+7 sec
2900 psi
@Temperature 1650 °F,
Time 10000 hour
 138 MPa
@Temperature 593 °C,
Time 3.60e+7 sec
20000 psi
@Temperature 1100 °F,
Time 10000 hour
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.300.30calculated
Shear Modulus 77.0 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000780 ohm-cm
@Temperature 20.0 °C
0.0000780 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.021.02at 200H
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.9 µm/m-°C
@Temperature 20.0 - 100 °C
8.83 µin/in-°F
@Temperature 68.0 - 212 °F
 17.1 µm/m-°C
@Temperature 20.0 - 500 °C
9.50 µin/in-°F
@Temperature 68.0 - 932 °F
 18.9 µm/m-°C
@Temperature 20.0 - 1000 °C
10.5 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  13.8 W/m-K
@Temperature 20.0 - 100 °C
95.8 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 18.7 W/m-K
@Temperature 20.0 - 500 °C
130 BTU-in/hr-ft²-°F
@Temperature 68.0 - 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.250 %<= 0.250 %
Chromium, Cr 24 - 26 %24 - 26 %
Iron, Fe 48 - 57 %48 - 57 %As Remainder
Manganese, Mn <= 2.00 %<= 2.00 %
Nickel, Ni 19 - 22 %19 - 22 %
Phosphorus, P <= 0.0450 %<= 0.0450 %
Silicon, Si <= 1.50 %<= 1.50 %
Sulfur, S <= 0.0300 %<= 0.0300 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
310 Stainless Steel, annealed sheet
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
310 Stainless Steel, annealed strip
Sandvik 310-7RE10 Billet

NL1004 / 17772

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.