MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Dielectric composition 7600A is a glass-ceramic insulative film designed for use in high density multilayer hybrid circuits using either gold or palladium-silver conductors. 7600A fires at 850°C to a smooth, dense, blue colored film that matches the thermal coefficient of expansion of alumina. Top gold conductor layers of Metech 3610 and 3612 exhibit excellent wire bonding using both aluminum and gold wire respectively. Top conductor layers of 3615 platinum-gold and 3504 palladium-silver display excellent solderability and aged adhesion.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 170000 - 190000 cP
@Temperature 25.0 °C
170000 - 190000 cP
@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Thickness 34.0 - 45.0 microns1.34 - 1.77 milFired
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmat 100VDC
Dielectric Constant 8.0 - 11
@Frequency 1000 Hz
8.0 - 11
@Frequency 1000 Hz
Dielectric Breakdown >= 600 V>= 600 VAC; 25 microns
Dissipation Factor <= 0.25
@Frequency 1000 Hz
<= 0.25
@Frequency 1000 Hz
 
Descriptive Properties
Coverage (cm²/gm)65-75Calculated from 50 micron wet film
Via Resolution (microns)200-250

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
712-3 Nextrema® Tinted Glass Ceramic/SCHOTT
724-5 Nextrema® Translucent White Glass Ceramic/SCHOTT
724-3 Nextrema® Transparent Glass Ceramic/SCHOTT
712-8 Nextrema® Opaque Grey Glass Ceramic/SCHOTT
712-6 Nextrema® Translucent Blue-Grey Glass Ceramic/SCHOTT

PLORD044 / 86052

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.