MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

724-3 Nextrema® Transparent Glass Ceramic/SCHOTT
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:
  • Very low coefficient of linear thermal expansion
  • Excellent temperature and thermal shock resistance
  • High transmission in infrared range and unique visible light transmission profiles with different specific grades
  • Excellent chemical resistance
High mechanical strength technical data presented herein are typical averages.

Vendors: NEXTREMA® glass-ceramics from SCHOTT combines the benefits of technical glasses with properties of high temperature materials.
General Brochure
Visit our web site and view the NEXTREMA® movies.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.54 g/cc0.0918 lb/in³
Porosity 0.00 %0.00 %ISO 9385
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 2.02.0DIN 12116
Alkali Class, AR 1.01.0ISO 695
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 570570HK 0.1 / 20; ISO 9385
Modulus of Elasticity 93.0 GPa13500 ksiASTM C-1259
Flexural Strength 135 MPa19600 psiBending sbB; DIN EN 1288, Part 5, R45
Poissons Ratio 0.250.25ASTM C-1259
Shear Modulus 37.2 GPa5400 ksiCalculated by MatWeb
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  200000 ohm-cm
@Temperature 350 °C
200000 ohm-cm
@Temperature 662 °F
DIN 52326
 4.00e+6 ohm-cm
@Temperature 250 °C
4.00e+6 ohm-cm
@Temperature 482 °F
DIN 52326
Dielectric Constant 7.8
@Frequency 1e+6 Hz,
Temperature 25.0 °C
7.8
@Frequency 1e+6 Hz,
Temperature 77.0 °F
DIN 53483
Dielectric Loss Index 0.019
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.019
@Frequency 1e+6 Hz,
Temperature 77.0 °F
DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear  -0.560 µm/m-°C
@Temperature -50.0 - 100 °C
-0.311 µin/in-°F
@Temperature -58.0 - 212 °F
 -0.540 µm/m-°C
@Temperature 0.000 - 50.0 °C
-0.300 µin/in-°F
@Temperature 32.0 - 122 °F
 -0.280 µm/m-°C
@Temperature 20.0 - 300 °C
-0.156 µin/in-°F
@Temperature 68.0 - 572 °F
 0.130 µm/m-°C
@Temperature 300 - 700 °C
0.0722 µin/in-°F
@Temperature 572 - 1290 °F
Specific Heat Capacity 0.800 J/g-°C
@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 1.60 W/m-K
@Temperature 90.0 °C
11.1 BTU-in/hr-ft²-°F
@Temperature 194 °F
DIN 51936, ASTM E 1461-01
Maximum Service Temperature, Air  560 °C
@Time 1.80e+7 sec
1040 °F
@Time 5000 hour
Inhomogeneous Heating
 710 °C
@Time 1.80e+7 sec
1310 °F
@Time 5000 hour
Homogeneous Heating
 750 °C
@Time 3600 sec
1380 °F
@Time 1.00 hour
Inhomogeneous Heating
 925 °C
@Time 3600 sec
1700 °F
@Time 1.00 hour
Homogeneous Heating
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.5415
@Wavelength 656.3 nm
1.5415
@Wavelength 656.3 nm
 1.542
@Wavelength 643.8 nm
1.542
@Wavelength 643.8 nm
 1.5445
@Wavelength 587.6 nm
1.5445
@Wavelength 587.6 nm
 1.5468
@Wavelength 546.1 nm
1.5468
@Wavelength 546.1 nm
 1.5513
@Wavelength 486.1 nm
1.5513
@Wavelength 486.1 nm
 1.5518
@Wavelength 180 nm
1.5518
@Wavelength 180 nm
 1.5566
@Wavelength 435.8 nm
1.5566
@Wavelength 435.8 nm
Transmission, Visible  66 %
@Thickness 4.00 mm,
Wavelength 400 nm
66 %
@Thickness 0.157 in,
Wavelength 400 nm
 87 %
@Thickness 4.00 mm,
Wavelength 600 nm
87 %
@Thickness 0.157 in,
Wavelength 600 nm
 90 %
@Thickness 4.00 mm,
Wavelength 700 nm
90 %
@Thickness 0.157 in,
Wavelength 700 nm
IR Transmittance  85 %
@Thickness 4.00 mm,
Wavelength 2500 nm
85 %
@Thickness 0.157 in,
Wavelength 2500 nm
 88 %
@Thickness 4.00 mm,
Wavelength 1600 nm
88 %
@Thickness 0.157 in,
Wavelength 1600 nm
 89 %
@Thickness 4.00 mm,
Wavelength 1000 nm
89 %
@Thickness 0.157 in,
Wavelength 1000 nm
 
Descriptive Properties
Abbé Value55.64546.1 nm
 55.89587.6 nm
Acoustical Characteristic, vlong.6600 m/s
AppearanceTransparent
ColorSlight Amber Hue
Hydrolytic Resistance HGB1DIN ISO 719
tk100(°C)175specific electric volume resistivity of 108 O·cm
Thermal Shock Resistance (TSR)820°CResists cold water without cracking

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
724-8 Nextrema® Opaque White Glass Ceramic/SCHOTT
712-3 Nextrema® Tinted Glass Ceramic/SCHOTT
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic
Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition
724-5 Nextrema® Translucent White Glass Ceramic/SCHOTT

CSGS803 / 178427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.