MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carlson Nitronic® 60® Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: General Description

Nitronic 60 is an anti-galling and wear resistant austenitic stainless steel. It provides a significantly lower cost alternative to combat wear and galling when compared with cobalt-bearing and high nickel alloys. The uniform corrosion resistance of Nitronic 60 is superior to 304 in most media. Chloride pitting resistance is superior to 316. Room temperature Nitronic 60 also possesses excellent high temperature oxidation resistance and low temperature impact resistance.

Due to its grain structure, the galling resistance of Nitronic 60 is superior to that of any other stainless steel. It resists wear, tearing or freeze up of both the primary and contact materials over a wide range of service temperatures. The elevated temperature wear resistance of Nitronic 60 is excellent despite its relatively low hardness when compared with cobalt and nickel-base wear alloys. It also performs well in metal-to-metal wear in nominally inert atmospheres. The cavitation erosion resistance of Nitronic 60 is superior to the austenitic stainless steels as well as high strength duplex (ferritic-austenitic) stainless steels.

The general corrosion resistance of Nitronic 60 falls between 304 and 316. However, in a wear system, a galling or seizure failure occurs first followed by dimensional loss due to wear and finally corrosion. Although the general corrosion resistance of Nitronic 60 is not as good as 316, it does offer better chloride pitting, stress corrosion cracking and crevice corrosion resistance.

In high temperature service, Nitronic 60 exhibits carburization superior to 316L and 309. Its oxidation resistance is far superior to 304 and 316 and comparable to 309.

Applications

  • Infrastructure bridge pin and hanger expansion joints, parking deck expansion joint wear plates.
  • Hydroelectric Power – stems, wicket gate wear rings
  • Oil and Gas Production – pump wear rings, bushings, valve trim, seals, fittings, logging equipment and screens.
  • Food processing and Pharmaceuticals – galling resistant applications in sanitary equipment where lubricants can not be used
  • Chemical and Petrochemical – process valve stems, seats and trim, pump wear rings.

Information provided by Carlson

Key Words: UNS S21800
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.62 g/cc0.275 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 241<= 241
Hardness, Rockwell B <= 100<= 100
Tensile Strength at Break 631 MPa91500 psiCarburized
 >= 655 MPa>= 95000 psi
Tensile Strength, Yield  >= 345 MPa
@Strain 0.2 %
>= 50000 psi
@Strain 0.2 %
 400 MPa
@Strain 0.2 %
58000 psi
@Strain 0.2 %
Carburized
Elongation at Break 19 %19 %Carburized; in 4xD
 >= 35 %>= 35 %
Reduction of Area 21.5 %21.5 %Carburized
Modulus of Elasticity 181 GPa26200 ksi
Taber Abrasion, mg/1000 Cycles 3.23.2vs. Nitronic 32
 6.06.0vs. 304
Bend Radius, Minimum 1.5 t1.5 tCarburized; 100°
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000982 ohm-cm0.0000982 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.8 µm/m-°C
@Temperature 25.6 - 93.3 °C
8.80 µin/in-°F
@Temperature 78.0 - 200 °F
 17.3 µm/m-°C
@Temperature 25.6 - 316 °C
9.60 µin/in-°F
@Temperature 78.0 - 600 °F
 18.5 µm/m-°C
@Temperature 25.6 - 649 °C
10.3 µin/in-°F
@Temperature 78.0 - 1200 °F
 19.8 µm/m-°C
@Temperature 25.6 - 982 °C
11.0 µin/in-°F
@Temperature 78.0 - 1800 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 59.13 - 65.42 %59.13 - 65.42 %
Manganese, Mn 7.0 - 9.0 %7.0 - 9.0 %
Nickel, Ni 8.0 - 9.0 %8.0 - 9.0 %
Nitrogen, N 0.080 - 0.18 %0.080 - 0.18 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si 3.5 - 4.5 %3.5 - 4.5 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed
MetalTek Nitronic® 60 Cast UNS J92972 Austenitic Stainless Steel
Carlson Nitronic® 50® Austenitic Stainless Steel
AISI Type S21800 Stainless Steel
321 Stainless Steel, annealed bar

NCARLSO09 / 15816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.